Product introduction
◆ Standards
316L Stainless Bar | GB | ASTM | JIS | ISO | EN |
022Cr17Ni12Mo2 00Cr17Ni14Mo2 |
S31603 316L |
SUS316L | X2CrNiMo17-12-2 |
X2CrNiMo17-12-2 1.4404 |
◆ Properties
Chemical composition of 316L stainless steel round bar | |||||||
C | Si | Mn | P | S | Ni | Cr | Mo |
≤0.030 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.030 | 10.00~14.00 | 16.00~18.00 | 2.00~3.00 |
Mechanical properties of 316L stainless steel square bar | |||||||
Yield Strength RP0.2/(N/mm2) |
Tensile Strength Rm/(N/mm2) |
Elongation after break A/% |
Rate of reduction in area Z/% |
HBW | HRB | HV | |
≥175 | ≥480 | ≥40 | ≥60 | ≤187 | ≤90 | ≤200 | |
Typical heat treatment regime for 316L stainless steel bar | |||||||
Solution treatment/℃ | 1010~1150,fast cooling | ||||||
Physical properties of 316L bar | |||||||
Density/(kg/dm³)20℃ | 8.00 | ||||||
Melting Range/℃ | - | ||||||
Specific Heat[kJ/(kg•K)]0℃~100℃ | 0.50 | ||||||
Thermal Conductivity/[W/(m•K)] | 100℃: 16.3; 500℃: 21.5 | ||||||
Coefficient of Thermal Expansion/(10-6/K) |
0℃~100℃:16.0; 0℃~500℃:18.5 |
||||||
Electrical Resistivity/(Ω•mm2/m)20℃ | 0.74 | ||||||
Modulus of Elasticity(kN/mm2)20℃ | 193 |